Unions claim incorrect welding procedure used in Gorgon repairs

AMWU also takes aim at state safety regulator for granting delay to inspection of the remaining two trains at giant LNG project

Union claim: the AMWU claims delays to repairs at Chevron's Gorgon LNG project have been due to the operator using an "incorrect welding procedure" to fix cracking on propane heat exchangers
Union claim: the AMWU claims delays to repairs at Chevron's Gorgon LNG project have been due to the operator using an "incorrect welding procedure" to fix cracking on propane heat exchangersPhoto: CHEVRON
Published 8 September 2020, 06:01Updated 8 September 2020, 08:26